LiTaO 3 crystal is also widely used E-O crystal, due to its optical, NLO and E-O poperties similar to those of LiNbO 3 crystal, but with higher damage threshold (> 500 MW/cm 2 for ns pulsed).
Transmitting range | 400 - 5200 nm |
Density | 7.46 g/cm 3 |
Melting Point | 1650 +/-5℃ |
Curie Point | 607 +/-5℃ |
Mohs Hardness | 5.5 |
Relative Dielectric Constant | e T11/e 0 : 85 e T33/e 0 : 29.5 |
Thermal Conductivity | 38 W /m /K @ 25℃ |
Dielectric Coefficient | e 11/E0:51.7 e33/E0:44.5 |
Coefficient:(x10 -11 C/m2) | CE11:2.77 |
Coefficient (x10 -11 C/N) | d22:0.8 |